. 2019 Mar 12;11(3):468. doi: 10.3390/polym11030468

Figure 7.

Figure 7

Evolution of generated temperature of the Ag NWs/PEDOT:PSS composite film with hexagonal and square pattern at (a) 12 V and (b) 54 V, respectively; On/off responses of the film heaters with hexagonal and square pattern at (c) 5 V and (d) 25 V, respectively.