Figure 20.

Figure 20

Molecular weight of produced phenyl silsesquioxanes with (a) initial concentration of PTMS, (b) water concentration, and (c) temperature of the reaction medium. Reprinted with permission from [29]. Copyright Elsevier, 2016.