Table 2.
References | Potentials | Method | Size | TC at 300 K (Wm−1 K−1) |
---|---|---|---|---|
Balandin (2008) [2] | / | Experiment | ~0.5–1 um | ~4840–5300 |
Wei (2011) [25] | AIREBO | RNEMD | 102 × 102Å2 | 77.3 |
Yang (2012) [26] | AIREBO | EMD | (90~270) × (40~180) Å2 | ~3200–5200 |
Xu (2014) [27] | Tersoff | NEMD | 50 × (2 × 150) Å2 | ~400–1800 |
Zhang (2012) [24] | AIREBO | RNEMD | 61 × 200 Å2 | ~170 |
This paper | AIREBO | NEMD | 60 × 200 Å2 | 182 |