Mixture proportions of cementitious geopolymer pastes for LDM applications.

Formulation ID Metakaolin (wt %) Alkaline Activator (wt %) Bentonite (wt %) Water (wt %) Spirulina platensis (wt %) Tetraselmis suecica (wt %) Lignin (wt %)
G-0 37.6 30.0 22.6 9.8 - - -
G-S1 37.0 29.5 22.2 10.6 0.6 - -
G-S3 36.2 28.9 21.8 11.4 1.7 - -
G-S5 35.5 28.3 21.3 12.1 2.8 - -
G-T1 37.0 29.5 22.2 10.6 - 0.6 -
G-T3 36.2 28.9 21.8 11.4 - 1.7 -
G-T5 35.5 28.3 21.3 12.1 - 2.8 -
G-L1 37.0 29.5 22.2 10.6 - - 0.6
G-L3 36.2 28.9 21.8 11.4 - - 1.7
G-L5 35.5 28.3 21.3 12.1 - - 2.8
U-S5 47.7 38.0 10.4 0.7 3.1 - -