Skip to main content
. 2019 Apr 2;12(7):1091. doi: 10.3390/ma12071091

Figure 16.

Figure 16

EDS X-ray elemental maps of a cross section of the alloy OHC5 after isothermal oxidation at 800 °C for 100 h, BSE image ×30,000.