Skip to main content
. 2019 Apr 2;12(7):1091. doi: 10.3390/ma12071091

Table 1.

Total weight gain, n values and oxidation rate constants of the alloys OHC1 and OHC5 after isothermal oxidation at 800 °C and 1200 °C.

Alloy and Temperature n kl (g·cm−2·s−1) kp (g2·cm−4·s−1) Weight Gain (mg/cm2)
OHC1-800 °C 0.89 3.9 × 10−9 > 10 h 5.47 × 10−13 (0–10 h) 1.42
OHC1-1200 °C 0.68 3.74 × 10−9 > 40 h 4.13 × 10−11 (0–40 h) 1.60
OHC5-800 °C 0.54 - 3.4 × 10−13 (0–1.3 h)
3.8 × 10−14 (1.3–24 h)
1.5 × 10−13 (>24 h)
0.22
OHC5-1200 °C - 4.4 × 10−8 (0–4.5 h)
2.1 × 10−8 (17–21.5 h)
1.41 × 10−12 (>21.5 h) 0.85