Table 1.

Standard deviation values corresponding to different test environments for three different types of metal depositions (electroplated gold electrode chip, evaporated gold electrode chip, sputtered gold electrode chip) (N = number of measurements).

Viscosity (m Pa.s) Test Condition Electroplated Gold Electrode Chip Std. Dev. Evaporated Gold Electrode Chip Std. Dev. Sputtered Gold Electrode Chip
Std. Dev.
1.60 RT 1× PBS 55 μA
N = 77
10 μA
N = 70
11 μA
N = 84
NA 3 °C 1× PBS 10 μA
N = 84
3 μA
N = 84
4 μA
N = 63
1.79 10% PBST 31 μA
N = 98
9 μA
N=105
4 μA
N = 56
1.83 10% GLYCEROL 31 μA
N = 77
10 μA
N = 84
9 μA
N = 63
6.83 50% GLYCEROL 21 μA
N = 77
7 μA
N = 84
4.27 μA
N = 70
262.4 90% GLYCEROL 13 μA
N = 84
4 μA
N = 70
4.16 μA
N = 70
782 100% GLYCEROL
(2.96)
56 μA
N = 84
28 μA
N = 91
33 μA
N = 63