Figure 4.

Figure 4

SEM images of the AgPtX modified SPCEs: (A) AgPtS@SPCE generated after 1 h, (B) AgPtL@SPCE generated after 1 h, (C) AgPtS@SPCE generated after 2.5 h, and (D) AgPtL@SPCE generated after 2.5 h of galvanic displacement.