Effect of mineralizers on ZrO2 crystallization using the hydrothermal method.

Mineralizer ZrO2 (300 °C, 24 h, 100 Mpa)
Tetragonal Monoclinic
KF (8 wt.%) No data 16 nm
NaOH (30 wt.%) No data 40 nm
H2O 15 nm 17 nm
LiCl (15 wt.%) 15 nm 19 nm
KBr (15 wt.%) 13 nm 15 nm