Figure 4

FESEM micrographs of scaffolds of HA fabricated with sintering temperature of 1200 °C and using different slurry solid content. (a) 20 wt.%HA, (b) 30 wt.%HA, (c) 40 wt.%HA; FESEM micrographs of scaffolds of HA with 20 wt.% of solid content and fabricated at different sintering temperature: (d) 1100 °C, (e) 1150 °C, (f) 1200 °C.