Figure 10.

Figure 10

FESEM micrographs of HA scaffolds after 30 days of soaking in SBF at different magnification. The scaffolds were sintered at 1200 °C and using (a) 20 wt.% of slurry solid content, (b) 40 wt.% of slurry solid content.