Table 1.

Acrylamide and bisacrylamide concentrations used to create varying elastic modulus PA gels.

Acrylamide Bisacrylamide Elastic modulus
7.5% 0.05% 6 kPa
10% 0.1% 14 kPa
10% 0.3% 29 kPa