Skip to main content
. 2019 Apr 24;6(4):181978. doi: 10.1098/rsos.181978

Table 2.

BET analysis results (indicating surface area and pore volume) of rGO samples synthesized at various drying temperatures with the corresponding data of graphite as reference.

BET surface area (m2 g−1) pore volume (cm3 g−1)
graphite 1.0293 0.0075
rGO-120 3.5581 0.0244
rGO-200 56.416 0.3088
rGO-250 148.89 0.812
rGO-300 148.32 0.7973