Skip to main content
. 2019 Apr 16;12(8):1246. doi: 10.3390/ma12081246

Figure 2.

Figure 2

Figure 2

Photomicrographs of hybrid ceramic (CERASMART™) before and after immersion in acidic drink for 7 and 28 days (40× magnification). (A,B) Before immersion; (C,D) after immersion in acidic drink for 7 days, (E,F) after immersion in acidic drink for 28 days.