Parameter Compressive Strength after 28 days Cement Water Sand 0–2 mm Aggregate above 2 mm
Codename cs_28 cement water fine_aggregate coarse_aggregate
Type target input input input input
Description The compressive strength of concrete 28 days after hydration. Considered as full strength. The weight of cement added to the mixture The weight of water added to the mixture The weight of sand added to the mixture The weight of aggregate, which have more than 2 mm, added to the mixture