Skip to main content
. 2019 Apr 17;12(8):1260. doi: 10.3390/ma12081260

Figure 8.

Figure 8

SEM image of failure surface of mortar specimens containing (a) 0% PCM, (b) 5% PCM, (c) 10% PCM, and (d) 20% PCM (BP = broken particles). Reprinted with permission from [91]. Elsevier (2015).