Skip to main content
. 2019 Mar-Apr;22(2):201–206. doi: 10.4103/JCD.JCD_485_18

Table 3.

Variation in bond strength of resin modified glass ionomer cement after application of various cavity cleansers

Groups n Bond strength mean (MPa) SD P Post hoc Tukey test
Group 1 (PAA) 8 8.9 4.6 <0.001 The significance was seen between
PAA and SDF-KI
CHX and SDF-KI
SDF-KI and CTRL
Group 2 (CHX) 8 9.7 5.3
Group 3 (SDF-KI) 8 22.3 4.4
Group 4 (CTRL) 8 10.5 10.5

CHX: 2% Chlorhexidine Gluconate, PAA: Polyacrylic acid, SDF: Silver diamine fluoride, KI: Potassium iodide, CTRL: Distilled water, SD: Standard deviation