Skip to main content
. 2019 May 13;5(5):e01703. doi: 10.1016/j.heliyon.2019.e01703

Table 2.

Vickers microhardness (HV) for composites obtained by various methods.

Molding method Vickers microhardness (HV)
Bi2O3, wt%
0 10 20 30 40 50 60
Cold pressing 42.2 48.3 57.2 62.9 66.9 73.0 76.6
Hot pressing 50.3 58.9 65.8 71.5 78.7 84.9 90.1