Skip to main content
. Author manuscript; available in PMC: 2019 May 17.
Published in final edited form as: Carbon N Y. 2011 Dec 2;50(4):1625–1634. doi: 10.1016/j.carbon.2011.11.043

Fig. 2.

Fig. 2

TGA of (a) MWCNTs alone, (b) CDDP alone and (c) MWCNT-CDDP. TGA are labelled with the wt.% of metal residue after ramping the sample to 1000 °C at a rate of 10 °C/min in air.