Skip to main content
. 2019 Apr 13;11(4):677. doi: 10.3390/polym11040677

Table 3.

Differential scanning calorimetry (DSC) results showing melting/crystallisation temperatures and melting enthalpies. Nascent crystallinity was calculated from the melting enthalpy using ∆H°m = 135.6 J/g [21].

Sample Tm1 (°C) Tc (°C) ΔHm1 (J/g) Xc %
PCL_A 57.2 36.4 92 67.8
PCL_F 62.7 35.7 105.2 77.6
PCL_I 61.9 34.1 102.7 75.7