Skip to main content
. 2019 Apr 3;11(4):609. doi: 10.3390/polym11040609

Figure 3.

Figure 3

(a) Maximum surface potential measured for a high number of repeated applications of virgin and used PA12 powders. (b) Relaxation of the electrostatic surface potential over time. Voltmeter probe has not been moved relatively to the powder layer in this measurement. Experiment has been conducted at 30% relative humidity.