Properties characterization of spinning solutions with the different weight ratio (polyethylene glycol:polylactide, or PEG:PLA).

PEG:PLA Electrical Conductivity (μs/cm) Viscosity (mPa·s)
1:1 0.455 ± 0.045 33 ± 2
1:3 0.432 ± 0.038 77 ± 4
1:5 0.421 ± 0.035 112 ± 3
1:7 0.267 ± 0.052 137 ± 3
1:9 0.249 ± 0.048 157 ± 4