Skip to main content
. 2019 Mar 28;10(4):221. doi: 10.3390/mi10040221

Figure 9.

Figure 9

A stroboscopic sequence of shadowgraph images showing the droplet ejection dynamics at pulse energy Ep = 2.5 µJ, process parameters: λ = 515 nm, film thicknesses dD = 9.52 µm liquid donor, and dPI = 3.5 µm polyimide.