Skip to main content
. 2019 Apr 29;12(9):1385. doi: 10.3390/ma12091385

Figure 5.

Figure 5

The SEM figures of Cr–Mn–Ni–N–Cu austenitic stainless steel samples treated at 750 °C for different times after the DL-EPR test: (a) 10 min; (b) 30min; (c) 60 min; (d) 120 min; (e) 300 min.