Figure 6.

Figure 6

The SEM figures of Cr–Mn–Ni–N–Cu austenitic stainless steel samples treated at different temperatures for 300 min after the DL-EPR test: (a) 600 °C; (b) 650 °C; (c) 700 °C; (d) 750 °C; (e) 800 °C.