Parameter PEH Type
HS-PEH SS-PEH
ΔPrms (mW) (at initial fr) −6.9% −23.6%
ΔPmax (mW) (at final fr) +0.20 −0.74
Δfr (Hz) −0.5 −0.8
NVPD (mW/cm3·Hz·g2) +7.9% −27.5%
Δdv (mm) (at initial fr) −0.04 −1.20
ΔC (nF) (at 100 Hz) +0.7% −2.1%
PS (μC/cm2) +4.7% −3.4%
Dielectric loss −16.2% +11.2%
Hysteresis loss +4.6% +20.6%
Mechanical loss (damping ratio) −0.3% +27.5%