Skip to main content
. 2019 May 7;12(9):1476. doi: 10.3390/ma12091476

Figure 4.

Figure 4

Mass loss of water through films of gluten plasticized with 35% of glycerol (A), 1,4-butanediol (B), and octanoic acid (C), with and without 20 php of microalgal biomass.