Skip to main content
. Author manuscript; available in PMC: 2020 May 28.
Published in final edited form as: Biomater Sci. 2019 May 28;7(6):2326–2334. doi: 10.1039/c9bm00020h

Fig. 3.

Fig. 3

Hydrophilicity of the SF films reflected by water static contact angle measurement. (a, c) Pristine SF film before (a) and after (c) mineralization. (b, d) Air-plasma-treated SF (A-SF) film before (b) and after (d) mineralization. The surface of air-plasma treated SF films was more hydrophilic than the other films.