Skip to main content
. 2019 May 14;52(Pt 3):587–598. doi: 10.1107/S160057671900342X

Figure 9.

Figure 9

Results of the FPSM analysis for the sample containing nanocrystalline periclase and large grains of calcite and magnetite. The magnetite is less than 3 wt% and not identified owing to the poor statistics on its intensities in addition to the small amount of content. The magnetite peaks are better fitted by the similar qandilite structure. Also, a spurious diamond phase was erroneously found. R wp: 0.151.