Skip to main content
. Author manuscript; available in PMC: 2020 Aug 1.
Published in final edited form as: J Mech Behav Biomed Mater. 2019 Apr 30;96:285–300. doi: 10.1016/j.jmbbm.2019.04.037

Table 2:

Theoretically and experimentally motivated bounds on GOH, SHR and FR model parameters and associated priors. Adapted from Table 1 in [10].

Model Parameter Constraint References Prior range
Material GOH & SHR (1 – ϕ)μ > 0 [0, 108]
GOH c1 > 0 [0,108]
GOH c2 >0 [0,103]
SHR ϕ E 0 – 14 GPa [34] [0, 108]
FR Ec >0 [10−3, 108]
FR Ee > 0 [10−3, 108]
Structural GOH k 0 – 1/3 [29] [0, 1/3]
GOH ξ 0 – π/2 [0, π/2]
SHR θ0 0 – π/2 [28] [10−3, π/2]
SHR ψ 0 – π/2 [0, π/2]
FR β 10 – 1000 [101, 103]