Skip to main content
. 2019 May 27;9(5):806. doi: 10.3390/nano9050806

Figure 2.

Figure 2

(A) Spectra of colloidal solutions of PANI/GOx composite nanoparticles synthesized at various solution pH values and (B) the influence of polymerization bulk solution pH on the absorbance at λmax = 440 nm. (The composition of polymerization solution: 0.05 mol L−1 of glucose, 0.50 mol L−1 of aniline and 0.75 mg mL−1 of glucose oxidase at pH 1.0–10; 48 h lasting polymerization was performed. Optical absorbance was registered in 0.05 mol L−1 SA buffer, pH 6.0).