. 2019 May 27;9(5):806. doi: 10.3390/nano9050806

Figure 4.

Figure 4

(A) Spectra of PTh/GOx composite nanoparticles colloidal solutions formed at various solution pH values and (B) dependence of optical absorbance at λmax = 450 nm on the solution pH. (The composition of polymerization solution: 0.05 mol L−1 of glucose, 0.50 mol L−1 of thiophene, and 0.75 mg mL−1 of glucose oxidase at pH 1.0–12; 48 h lasting polymerization was performed. Optical absorbance was registered in 0.05 mol L−1 SA buffer, pH 6.0).