. 2019 May 27;9(5):806. doi: 10.3390/nano9050806

Table 1.

The dependence of PANI/GOx, Ppy/GOx, and PTh/GOx composite nanoparticles diameter on the pH of solutions. The composition of polymerization solution: 0.05 mol L−1 of glucose, 0.75 mg mL−1 of GOx and 0.50 mol L−1 of aniline, pyrrole, or thiophene. The particles were formed by 48 h lasting enzymatic polymerization. The diameter of particles was determined by dynamic light scattering (DLS) in 0.05 mol L−1 SA buffer, pH 6.0.

pH Diameter, nm
PANI/GOx Ppy/GOx PTh/GOx
2.0 180 ± 94 180 ± 46 169 ± 62
5.0 56 ± 22 155 ± 61 63 ± 9.4
6.0 54 ± 6.9 86 ± 18 98 ± 28
8.0 106 ± 41 308 ± 49 535 ± 106