(a) XRD results of PET and laser-welded AgNW FTCFs. (b) Plot of the sheet resistance versus time for laser-welded AgNW FTCFs after exposure to humid and hot air (humidity: 85%, temperature: 85 °C) for 30 days. Inset: the morphology of nanowire after the end of the 30-days stability test. R0 is the initial resistance, Ra is the resistance measured after the experiment.