Skip to main content
. 2019 May 2;11(5):787. doi: 10.3390/polym11050787

Figure 2.

Figure 2

DSC curves from heating: (a) Heating from −150 °C to 170 °C and (b) two heating scans from −100 °C to 150 °C.