Skip to main content
. 2019 May 10;11(5):848. doi: 10.3390/polym11050848

Figure 3.

Figure 3

Surface hydrophobicity (H0) of BBPI by wet heating and ultrasound treatment Maillard reaction obtained for 1–6 h, respectively. Means with dissimilar lower-case letters indicate significant differences (p < 0.05), ** means in the same time p < 0.01, * means in the same time p < 0.05.