Skip to main content
. 2019 May 26;11(5):922. doi: 10.3390/polym11050922

Figure 4.

Figure 4

FT-IR spectra of EVOH and EVOH_ ZnO Nrods at different ZnO contents at time 0 (a), and after different exposition times (5 and 10 days) of accelerated-aging test for EVOH (b), EVOH_0.1ZnO Nrods (c) and EVOH_1ZnO Nrods (d).