Skip to main content
. 2019 May 23;11(5):916. doi: 10.3390/polym11050916

Figure 3.

Figure 3

Features of 12% and 15% ES-PLA scaffolds. Images taken from the top and bottom sides were used to calculate (a) fiber diameter, (b) surface porosity, and (c) pore diameter. Results are shown as average ± SE. SF: small fibers; LF: large fibers.