Skip to main content
. 2019 Jun 14;5(6):e01489. doi: 10.1016/j.heliyon.2019.e01489

Fig. 5.

Fig. 5

FE- SEM micrographs of MgFe2-xCexO4 (x = 0.04, 0.08, 0.12) at different sintering temperatures and material fabrication. a-c1: pellet samples, d-f1: Thick film samples.