. 2019 Jun 14;5(6):e01489. doi: 10.1016/j.heliyon.2019.e01489

Table 2.

Energy Dispersive X-ray analysis of MgFe2-xCexO4 (x = 0.04, 0.08, 0.12) samples sintered at 973 K.

Element MgFe1.96Ce0.04O4
MgFe1.92Ce0.08O4
MgFe1.88Ce0.12O4
Pellets
Thick films
Pellets
Thick films
Pellets
Thick films
Wt (%) At (%) Wt (%) At (%) Wt (%) At (%) Wt (%) At (%) Wt (%) At (%) Wt (%) At (%)
O 20.35 42.45 17.50 38.72 21.58 45.05 18.31 40.43 18.98 41.99 19.11 42.28
Mg 13.95 19.17 12.59 18.35 13.45 18.47 12.66 18.38 12.41 18.08 12.38 18.02
Ce 2.48 0.59 3.59 0.91 6.62 1.59 6.46 1.64 9.37 2.38 9.81 2.47
Fe 63.22 37.79 66.32 42.02 58.35 34.89 62.55 39.55 59.24 37.55 58.70 37.23