Skip to main content
. 2019 Jun 12;10:1298. doi: 10.3389/fmicb.2019.01298

FIGURE 11.

FIGURE 11

Potentiodynamic polarization curves of specimens covered with deposit in the absence and presence of SRB after 14 days of incubation in CO2-saturated simulated formation water.