Skip to main content
. 2019 Jun 21;9:9012. doi: 10.1038/s41598-019-45439-x

Figure 5.

Figure 5

(a) Difference and (b) DSC image of the PS particles with the mean diameter of 50 nm (c) lineprofile corresponding to green line cut in (a) and (b). (d) SNR distribution of detected particles in both methods. (e) Particle SNR comparison for both methods. 2 µm defocus range is used in the analysis. Scalebar is 5 µm.