Figure 8.
(a) 13 and 20 nm NRs used to build up Pb0.81Ag0.16K0.03Te0.33S0.67 and Pb0.89Ag0.10K0.01Te0.28S0.72 nanocomposites, respectively, and the corresponding (b) electrical conductivity, σ, and (c) Seebeck coefficient, S.
(a) 13 and 20 nm NRs used to build up Pb0.81Ag0.16K0.03Te0.33S0.67 and Pb0.89Ag0.10K0.01Te0.28S0.72 nanocomposites, respectively, and the corresponding (b) electrical conductivity, σ, and (c) Seebeck coefficient, S.