Skip to main content
. 2019 May 30;12(11):1756. doi: 10.3390/ma12111756

Figure 2.

Figure 2

(a) Log stress-Log strain rate curves at a temperature range of 700 °C–900 °C obtained by a tensile test with step-by-step increment techniques. (b) The strain rate sensitivity index m.