(A) Photothermal conversion curves of water and MnO2-PEG-cRGD/Ce6 nanoparticles at different concentrations upon irradiation with an 660 nm laser (0.6 W cm − 2). (B) Photothermal conversion curves of MnO2-PEG-cRGD/Ce6 nanoparticles (100 µg mL − 1) at different laser power densities. (C) Photothermal conversion stability of MnO2-PEG-cRGD/Ce6 nanoparticles. The laser was turned on for 10 min and then turned off for each cycle. (D) Linear relationship between time and − ln θ calculated from cooling period after the laser was turned off.