Skip to main content
. 2019 May 4;4:100032. doi: 10.1016/j.wroa.2019.100032

Table 3.

Aqueous concentrations of metals (μg/l)) after initial leaching tests.

Material Cd Cr Cu Ni Pb Zn
LTU-TOP <0.05 1.63 4.64 1.07 1.34 3.76
Hekla <0.05 <0.5 10.01* 2.44 1.93 15.6*
Hekla-B <0.05 <0.5 7.68* 1.985 1.34 13.1*
DWA <0.05 <0.5 <1 <0.5 <0.2 <2
DWA-chalk <0.05 <0.5 <1 <0.5 <0.2 <1
Hasselfors <0.05 <0.5 4.4 <0.5 0.45 3.19
NC-USA <0.05 <0.5 1.72 <0.5 0.88 <2
KB-OHIO <0.05 <0.5 3.27 2.17 <0.1 <2
BN-OHIO <0.05 <0.5 6.16 4 <0.2 <2
Orbicon <0.05 <0.5 3.37 0.56 0.24 <2
Control <0.05 <0.5 1.82 <0.5 <0.2 2.31

Values with < below detection limit. *significantly higher than control (one-way ANOVA with Tukeys comparison).