. 2019 May 5;10(2):20. doi: 10.3390/jfb10020020

Table 3.

Refined structural parameters for ZnTCP samples.

M 1 5ZnTCP 10ZnTCP
OF Sr  atoms/cell
M(1) 18 0.05 0.9 0.03 0.5
M(2) 18 0.07 1.3 0.07 1.2
M(3) 18 0.07 1.3 0.08 1.4
M(4) 2 6 0.05 0.0 0.03 0.0
M(5) 6 0.15 0.9 0.97 5.8
Zn at/cell 3 - 4.4 8.9
Zn at% 4 - 7.0 14.1
Rwp (%) - 7.4 8.9

1 multiplicity of crystal site; 2 the overall content of site 4 is 0.43; 3 total metal atoms inside unit cell are 63.2 [15]; 4 from refinement.