(a) Cyclic voltammetry in H2O + 5 mM CuSO4 + 0.1 M LiClO4 at glassy carbon, scan rate 0.2 V·s−1; (b) double potential pulse for the Cu deposition applied in this study. Adapted with permission from Durante et al. [254]. Copyright (2014), John Wiley and Sons.