DOX loading efficiency (DLEDOX) and DOX loading content (DLCDOX) and equivalent values for AuNR loadings calculated for the obtained polymersomes.

Polymersome DLEDOX (%) LEAuNR a (%) DLCDOX (%) LCAuNR b
P51D47 52.0 - 12.0 -
P51D47@AuNR-761 47.4 44.7 10.9 16.1
P122D54 46.7 - 10.8 -
P122D54@AuNR-761 44.3 42.5 10.2 15.3
P122D96 48.3 - 11.1 -
P122D96@AuNR-761 44.7 33.8 10.3 12.2

a Loading efficiency of AuNR (LEAuNR) as determined by Equation (1) but using data from AuNR. b Loading content of AuNR (LCAuNR) as determined by TGA analysis, subtracting the residue from the block copolymers to those of the PEGm-b-PDEAEMn@AuNR materials.