Table 1.

Details of solution preparation for electrospinning and spin-coating of poly(methyl methacrylate) (PMMA) including—molecular weight (Mw), concentration w/w (C), solvents, and the rotation speed of stirrer (Vr); the electrospinning parameters—voltage (U), distance needle to collector (d), flow rate (Q), and humidity (H), used to produce PMMA scaffolds with nanofibers, microfibers, and ribbons.

PMMA Scaffold Solution Preparation Electrospinning Parameters
Mw [g·mol−1] Solvent C [%] vr [rpm] U [kV] d [cm] Q [mL·h−1] H [%]
Nanofibers 150,000 Formic Acid: DMF 7:3 12 500 11 10 0.3 40
Microfibers 150,000 DMF 30 750 12 15 3 40
Ribbons 350,000 Formic Acid 12 500 13 15 0.6 45
Film 350,000 DMF 12 500 - - - -